ERNiFeCr-2/UNS N07718/W.Nr. 2.4668 AWS A5.14 Wire
Overview
Limiting Chemical Composition, %
Nickel..................................................................................................................................................................................50.00-55.00
Chromium...........................................................................................................................................................................17.00-21.00
Molybdenum...........................................................................................................................................................................2.80-3.30
Niobium...................................................................................................................................................................................4.75-5.00
Titanium..................................................................................................................................................................................0.65-1.15
Manganese.............................................................................................................................................................................0.35 max.
Iron......................................................................................................................................................................................11.95-24.80
Silicon......................................................................................................................................................................................0.35 max.
Aluminium........................................................................................................................................................................0.20-0.80max.
Carbon.....................................................................................................................................................................................0.08 max.
Phosphorous.........................................................................................................................................................................0.015 max.
Sulfur....................................................................................................................................................................................0.0015 max.
Cobalt.......................................................................................................................................................................................1.00 max.
Physical properties
Melting point Co |
Coefficient of Expansion.21-9 Co,μm/m*Co |
Electrical Resistivity, μQ*m |
Density g/cm3 |
1260-1336 |
13.0 |
1.25 |
8.19 |
Mechanical Properties
Tensile strength MPa(psi) |
Elongation A % |
1138(165,000) |
≥25 |
Corrosion Resistance
Corrosion can be an unrelenting foe in various industrial settings. ErNiFeCr-2’s outstanding corrosion resistance is a testament to its longevity and reliability, even in highly corrosive conditions. This attribute is paramount in marine and chemical processing applications.
High-Temperature Performance
ErNiFeCr-2 filler metal is well-suited for high-temperature applications in various industries, including power generation, heat treatment, and metal refining. The welds produced with this filler metal can withstand prolonged exposure to elevated temperatures without significant loss of mechanical strength or corrosion resistance.
Heat treatment
Product Forms And Packaging (0ther sizes available -please contact us)
Product |
Diameter |
Length |
Packaging |
Wire For MIG/GMAW Welding |
0.8mm/1.0mm/1.2mm/1.6mm/2.0mm/2.4mm /2.5mm/3.2mm |
- |
33 lbs (15kgs) |
Rods For TIG/GTAW Welding |
2.0mm /2.4mm /2.5mm/3.2mm/4.0mm/5.0mm |
915mm-1000mm |
11 lbs (5kgs) |
Wire For SAW Welding |
2.0mm /2.4mm /2.5mm /3.2mm /4.0mm/5.0mm |
- |
60 lbs (27kgs) |