Refractory 26/Alloy R26/W.Nr.1.2888 Pipe Wire Foil Strip Sheet
Overview
Alloy R26 is Fe – NI – Co – Cr precipitation hardening type deformation of high temperature alloy, long-term use of C – 570 °C temperature range of 540 °C, the highest temperature can reach 677 C, add element of a Cr, mo alloy solid solution strengthening, high to low titanium, aluminum form y aging strengthening phase, while drilling elements made of titanium, aluminum solubility in the solid solution is reduced, prompted y phase precipitation amount increase, so as to improvel the thermal stability of y, reduce y ‘phase of the stacking fault energy.
The nickel-based refractory R26 combines excellent creep resistance and good hot chemical properties. Its characteristics make it a preferred candidate for the most difficult applications.
Limiting Chemical Composition, %
Nickel..................................................................................................................................................................................35.00-39.00
Chromium...........................................................................................................................................................................16.00-20.00
Cobalt..................................................................................................................................................................................16.00-22.00
Iron........................................................................................................................................................................................9.65-26.60
Manganese.............................................................................................................................................................................0.40-1.00
Carbon....................................................................................................................................................................................0.08 max.
Silicon.....................................................................................................................................................................................0.50-1.50
Boron.....................................................................................................................................................................................0.001-0.01
Sulphur....................................................................................................................................................................................0.03 max.
Phosphorus.............................................................................................................................................................................0.03 max.
Molybdenum...........................................................................................................................................................................3.00-3.40
Thallium..................................................................................................................................................................................2.50-3.00
Aluminium...............................................................................................................................................................................0.30 max.
Physical properties
Density |
Melting range |
9.14g/cm³ |
1300-1330°C |
Mechanical Properties
Tensile Strength (σb/MPa) |
Yield Strength (σp0.2/MPa) |
Elongation (σ5/%) |
1000 |
550 |
15 |
Heat-Treatment
Refractory 26 heat treatment includes solution treatment and aging treatment. The temperature of solution treatment is 1025℃, and rapid cooling is required. Aging treatment includes water cooling after 20 hours at 815 ° C and air cooling after 20 hours at 730 ° C.
Available Forms
We provide you with a variety of product forms, including but not limited to.
● Strips & Tape
● Wire & Welding
● Pipe & Tube
● Sheet & Foils
● Flanges & Forgins